ISO 5618-2:2024
Current
The latest, up-to-date edition.
Fine ceramics (advanced ceramics, advanced technical ceramics) — Test method for GaN crystal surface defects — Part 2: Method for determining etch pit density
Hardcopy , PDF , PDF 3 Users , PDF 5 Users , PDF 9 Users
English, French
04-30-2024
This document describes a method for determining the etch pit density, which is used to detect dislocations and processing-introduced defects that occur on single-crystal GaN substrates or single-crystal GaN films.
It is applicable to the defects specified in ISO 5618-1from among the defects exposed on the surface of the following types of GaN substrates or films: single-crystal GaN substrate; single-crystal GaN film formed by homoepitaxial growth on a single-crystal GaN substrate; or single-crystal GaN film formed by heteroepitaxial growth on a single-crystal Al2O3, SiC, or Si substrate.
It is applicable to defects with an etch pit density of ≤ 7 × 107cm-2.
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.